Effect of Ruthenium on Creep Strength of Ni-Base Single-Crystal Superalloys at 750

โœ Scribed by N. Tsuno; K. Kakehi; C.M.F. Rae; R. Hashizume


Book ID
107443722
Publisher
The Minerals, Metals & Materials Society
Year
2008
Tongue
English
Weight
522 KB
Volume
40
Category
Article
ISSN
1073-5623

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Anisothermal creep behavior at very high
โœ J. Cormier; X. Milhet; J. Mendez ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 438 KB

Nickel-based superalloy single crystal specimens have been tested under anisothermal creep conditions using two different routes, both including an overheating stage. In the first route, the material is tested under creep conditions at 1050 โ€ข C, then submitted to an overheating regime at 1200 โ€ข C, a