Crack-healing and mechanical behaviour of Al2O3/SiC composites at elevated temperature

โœ Scribed by K. ANDO; B.-S. KIM; M.-C. CHU; S. SAITO; K. TAKAHASHI


Book ID
109013976
Publisher
John Wiley and Sons
Year
2004
Tongue
English
Weight
405 KB
Volume
27
Category
Article
ISSN
8756-758X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Bending strength and crack-healing behav
โœ Hae Sook Kim; Mi Kyung Kim; Sun Bae Kang; Seok Hwan Ahn; Ki Woo Nam ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 665 KB

Five kinds of ceramics were used to evaluate the bending strength under three-point bending. The bending test was carried out at room temperature. The crack-healing behavior and the bending strength of the crack-healed specimens were investigated from room temperature to 1723 K. The bending strength

Fracture behaviour of Al2O3/SiC nanocomp
โœ Zdenek Chlup; Petr Flasar; Ando Kotoji; Ivo Dlouhy ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 769 KB

The self-crack-healing ability was systematically studied using flexural strength measurement of beams containing a semi-elliptical surface crack made by Vickers indenter. Beams of Al 2 O 3 /SiC ceramic nanocomposite with a good self-crack-healing ability predetermined for four-point and three-point

Elevated temperature fracture resistance
โœ M.G. Jenkins; A.S. Kobayashi; K.W. White; R.C. Bradt ๐Ÿ“‚ Article ๐Ÿ“… 1988 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 919 KB

The fracture resistance of a Sic whisker/AlzO, matrix composite for the test temperature range of 20" to 1400ยฐC was determined using chevron-notched and straightnotched, three-point bend specimens. Crack mouth opening displacement (CMOD) was continuously monitored throughout the fracture tests, usin