Corrosion of technical ceramics by molten aluminium
โ Scribed by U. Schwabe; L.R. Wolff; F.J.J. van Loo; G. Ziegler
- Publisher
- Elsevier Science
- Year
- 1992
- Tongue
- English
- Weight
- 780 KB
- Volume
- 9
- Category
- Article
- ISSN
- 0955-2219
No coin nor oath required. For personal study only.
โฆ Synopsis
Corrosion investigations with various types o[ nonoxide technical ceramics, eight silicon nitride materials (1 grade of HIPRBSN, 3 grades of HPSN and 4 grades of RBSN), and two O'pes o[ silieon carbide (HIPSiC and SiSiC) were carried out h7 alumhlium melts (pure aluminium and AIZnMgCul'5). HIPRBSN and HPSN materials exhibit near O, no corrosion attack under the most severe conditions applied ( lO00ยฐC for 750h). RBSN materials with relatively high open porosity are attacked after relatively short times. HIPSiC is considerably more attacked than HIPRBSN and the HPSN materials: however, it is also fairly corrosion resistant. SiSiC reveals the poorest corrosion behaviour of the materials investigated. The results are explained in terms ~[ thermodynamics, d(ffhsion through the metal[ceramic interjaee and wetting ~tJ'e c t s.
๐ SIMILAR VOLUMES
Titanium diboride TiB ceramic particulates are dispersed in molten aluminium and its alloys for grain 2 refining and for making cast metal1matrix composites. For producing cast MMC, the dispersion of the ceramic phase via in-situ aluminothermic reduction of K TiF and KBF flux mixture with molten 2 6
The aluminium alloys exhibit, when submitted to certain aggressive conditions, a particular corrosion feature named exfoliation, leading to the formation of thin laminar corroding foils. Three different alloys having distinct corrosion features; 2024 T351, 2219 T87 and 6013 T6 were immersed in the E