## Abstract Corrosion fatigue and fatigue properties of spot‐welded austenitic stainless steels EN 1.4301 and EN 1.4318 in 2B or 2F and 2H conditions were investigated in 3.5% sodium chloride (NaCl) solution and in air. The shear‐loaded specimens were single spot overlap joints. The effect of stee
Corrosion fatigue of welded offshore steels and tubular connections
✍ Scribed by W.J. Oberparleiter
- Publisher
- Elsevier Science
- Year
- 1985
- Tongue
- English
- Weight
- 704 KB
- Volume
- 4
- Category
- Article
- ISSN
- 0167-8442
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract Tubular space trusses for bridge applications use thick‐walled tubes. The reduction in fatigue resistance due to geometrical size effects is thus an important issue. In order to carry out a thorough study, both fatigue tests on large‐scale specimens and advanced 3D crack propagation mod
## Abstract Corrosion fatigue and fatigue properties of weld‐bonded and spot‐welded austenitic stainless steels EN 1.4301 and EN 1.4318 in 2B or 2F and 2H conditions were investigated. The corrosive environment was 3.5% NaCl solution at + 50 °C. In air the fatigue strengths of the weld‐bonded singl
## Abstract The corrosion resistance of spot‐welded and induction‐heated austenitic stainless steels EN 1.4301 and EN 1.4318 was investigated in 3.5% sodium chloride solution at ambient temperature. In potentiostatic measurements pitting corrosion of spot‐welded and induction‐heated samples occurs
This paper presents the fatigue results obtained in two types of stainless steels: Duplex S31803 and Austenitic 304L. The main objective was to compare the fatigue behavior in terms of environment (air and 3% NaCl) and weld toe treatment (as welded and toe grinding). The tests were carried out in te