Corrosion and inhibition of stainless steel pitting corrosion in alkaline medium and the effect of Cl− and Br− anions

✍ Scribed by S.A.M. Refaey; F. Taha; A.M. Abd El-Malak


Publisher
Elsevier Science
Year
2005
Tongue
English
Weight
267 KB
Volume
242
Category
Article
ISSN
0169-4332

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Corrosivity of Br− and Cl− on duplex sta
✍ Katsumi Yamamoto; Keizo Hosoya 📂 Article 📅 1995 🏛 Elsevier Science 🌐 English ⚖ 385 KB

This report discusses the basis for material selection in chemical plants, especially focusing on the design of an actual plant based on laboratory corrosion test results. Both the chemical system created when chlorine gas and bromine gas were neutralized with alkaline solution, and material economi

Effect of biomineralized manganese on pi
✍ B. H. Olesen; N. Yurt; Z. Lewandowski 📂 Article 📅 2001 🏛 John Wiley and Sons 🌐 German ⚖ 161 KB

During the past few years, biomineralized manganese has been shown to cause ennoblement of various stainless steels to open circuit potentials of 300 ± 400 mV/SCE. We have demonstrated that ennoblement, caused by biologically deposited manganese minerals, along with a relatively low stainless steel

Pitting corrosion behavior of superferri
✍ G. Moretti; G. Quartarone; A. Tassan; A. Zingales 📂 Article 📅 1993 🏛 John Wiley and Sons 🌐 German ⚖ 674 KB

## Abstract On a cost‐performance basis, superferritic stainless steel (SFSS) grades can now be considered competitive choices for brackish and sea water cooling systems. The pitting corrosion of a SFSS (X2CrNiMoTi 25 3.6 3.5) was tested in a chloride/sulfate solution similar to sea water, as a fun

An investigation on the effect of bleach
✍ M. H. Moayed; M. Golestanipour 📂 Article 📅 2005 🏛 John Wiley and Sons 🌐 German ⚖ 231 KB 👁 1 views

Pitting corrosion and transpassive dissolution of 316 stainless steel in a solution containing five percent of commercial bleaching liquid was investigated by employing potentiodynamic polarization method and recording corrosion potential during immersion. Today commercial bleaching liquids are wide