📜 SIMILAR VOLUMES
TiO 2 films were grown on carbon fiber by atomic layer deposition (ALD), and adsorption and photocatalytic decomposition of methylene blue (MB) on these TiO 2 films were studied. They showed very high adsorption capacities of MB, indicating that these films can be used as adsorbents for removing org
## Abstract The effect of heat treatment on the gas barrier of the polymer‐coated board further coated with an Al~2~O~3~ layer by atomic layer deposition (ALD) was studied. Heat treatment below the melting point of the polymer followed by quenching at room temperature was used for the polylactide‐c