Atomic Layer Deposition of Conductive Coatings on Cotton, Paper, and Synthetic Fibers: Conductivity Analysis and Functional Chemical Sensing Using “All-Fiber” Capacitors
✍ Scribed by Jesse. S. Jur; William J. Sweet III; Christopher J. Oldham; Gregory N. Parsons