Characterization of the impact of plasma treatments and wet cleaning on a porous low k material
✍ Scribed by W. Puyrenier; V. Rouessac; L. Broussous; D. Rébiscoul; A. Ayral
- Publisher
- Elsevier Science
- Year
- 2006
- Tongue
- English
- Weight
- 271 KB
- Volume
- 83
- Category
- Article
- ISSN
- 0167-9317
No coin nor oath required. For personal study only.
✦ Synopsis
In the back end of line (BEOL) interconnections for 65 nm and beyond technology nodes, the integration of porous low dielectric constant (low k) materials is now needed to improve signal propagation. Porosity in low k films drives new challenges concerning the different steps of the integration. Thus, the characterization of porosity is needed to develop and optimize low k dielectric films, but also to characterize process steps that may impact the porosity: etch and cleaning processes. In this paper, the impact of several plasma treatments and wet cleaning process on the dielectric material were characterized. All the plasma treatments tested lead to the formation of a thin and dense layer at the material surface with different porosities (pore sealing or open porosity). The cleaning compatibility depends on this thin zone: pore sealing limits water-uptake but can lead to increase the dielectric constant.
📜 SIMILAR VOLUMES
The impact of material / process interactions on low temperature CVD-O low-k dielectric film properties are 3 presented. The film under investigation is deposited following a three-step process consisting of a low temperature chemical vapor deposition (CVD), an ex situ high temperature cure in a con
With the advent of novel therapies for Alzheimer's disease, there is pressing need for biomarkers that are easy to monitor, such as the amyloid-beta (A beta) levels in the cerebrospinal fluid (CSF) and plasma. To gain a better understanding of the explanatory power of these biomarkers, we formulate
## Abstract An accelerated anodic corrosion method was used to study the effects of heat treatment and bead size on corrosion and metal ion release of porous coated F75 cylinders in saline and serum. Three heat treatments were used: a standard process for F75 implants (HTA), the standard plus an ad