Acoustic emission of fatigue crack in pressure pipe under cyclic pressure

โœ Scribed by Qiong Ai; Cai-Xue Liu; Xiang-Rong Chen; Pan He; Yao Wang


Publisher
Elsevier Science
Year
2010
Tongue
English
Weight
704 KB
Volume
240
Category
Article
ISSN
0029-5493

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Fatigue fracture analysis of spherical s
โœ Sadia M. Makky ๐Ÿ“‚ Article ๐Ÿ“… 1988 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 255 KB

The ultimate strength and endurance limit for a spherical container under internal pressure have been analytically determined. In addition, the number of cycles that may cause fracture of the container due to fatigue is found as a function of the peak of the cyclic pressure, the inner and the outer

Hydrogen diffusion analyses of a cracked
โœ K. Takayama; R. Matsumoto; S. Taketomi; N. Miyazaki ๐Ÿ“‚ Article ๐Ÿ“… 2011 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 769 KB

In hydrogen diffusion in metals, we have to consider not only the hydrogen flux driven by the gradient of hydrogen concentration but also the hydrogen flux driven by the gradient of hydrostatic stress. Such hydrogen diffusion is a multi-physics problem coupled hydrogen diffusion with a stress field.