A new blue-emitting phosphor LiCaPO 4 :Eu 2+ was synthesized by solid state reaction at a relatively low temperature of 900 °C. It gives a single intense emission band centering at 470 nm, which corresponds to the 4f 6 5d 1 → 4f 7 transition of Eu 2+ . The dependence of luminescence intensities on E
Ultraviolet Pumped Tricolor Phosphor Blend White Emitting LEDs
✍ Scribed by Kaufmann, U. ;Kunzer, M. ;K�hler, K. ;Obloh, H. ;Pletschen, W. ;Schlotter, P. ;Schmidt, R. ;Wagner, J. ;Ellens, A. ;Rossner, W. ;Kobusch, M.
- Publisher
- John Wiley and Sons
- Year
- 2001
- Tongue
- English
- Weight
- 264 KB
- Volume
- 188
- Category
- Article
- ISSN
- 0031-8965
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
A novel blue-emitting phosphor, LiSrPO 4 :Eu 2+ , was prepared by the solid-state reaction and X-ray powder diffraction (XRD) analysis confirmed the formation of LiSrPO 4 :Eu 2+ . Photoluminescence (PL) results showed that the phosphor can be efficiently excited by UV-visible light from 250 to 440 n
Blue-Emitting Phosphor M 2 B 5 O 9 Cl: Eu 2+ (M: Sr, Ca) for White LEDs. -The title phosphors are prepared by solid state reaction of stoichiometric amounts of SrCO3 or CaCO3, SrCl2 or CaCl2 (5% excess), H3BO3 (10% excess), and Eu2O3 (corundum crucible, 900 °C, 4 h). The luminescence properties of t
## Abstract ChemInform is a weekly Abstracting Service, delivering concise information at a glance that was extracted from about 200 leading journals. To access a ChemInform Abstract of an article which was published elsewhere, please select a “Full Text” option. The original article is trackable v
0.54 Sr 0.46À1.5xÀ1.5z Eu z Gd x (MoO 4 ) y (WO 4 ) 1Ày LED Red-emitting phosphors a b s t r a c t A series of Eu 3+ -Gd 3+ co-doped solid solution of Ca 0.54 Sr 0.46-1.5x-1.5z Eu z Gd x (MoO 4 ) y (WO 4 ) 1Ày (x=0.01-0.20, y=0-1.0, z=0.01-0.30) have been prepared by solid-state reactions. It is fou