𝔖 Bobbio Scriptorium
✦   LIBER   ✦

The use of “Boersma” type differential scanning calorimeters in the measurement of exothermic transitions

✍ Scribed by S. Dallek; L. Kabacoff


Publisher
Elsevier Science
Year
1982
Tongue
English
Weight
391 KB
Volume
57
Category
Article
ISSN
0040-6031

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Modeling of the heat-transfer process in
✍ B. Sen 📂 Article 📅 1992 🏛 American Institute of Chemical Engineers 🌐 English ⚖ 546 KB

## Abstract The model developed predicts a priori potential errors associated with the energy trace recorded by an isoperibol differential power scanning calorimeter in the measurement of heat of adsorption of H~2~ on Pt and Pd catalysts. The uptake of H~2~ by the catalyst sample was approximated b