The shear band stress-corrosion cracking of an aluminium-lithium alloy
โ Scribed by Y. L. Shen; J. J. Chan; S. C. Chang
- Publisher
- Springer
- Year
- 1988
- Tongue
- English
- Weight
- 165 KB
- Volume
- 7
- Category
- Article
- ISSN
- 0261-8028
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
The stress corrosion cracking behaviour of plate material of the aluminium alloys 2024-T351, 8090-T8171, 7475-T651, and 7075-T7351 was investigated performing constant load tests. Short transverse tensile specimens were permanently immersed in aerated aqueous 0.6 M Na 2 Cl solutions with additions o
A fracture mechanics approach to stress corrosion cracking is highlighted. The mechanisms of stress corrosion cracking is presented. Experiments on 2024 and 7075 aluminium alloys are carried out to determine their mechanical properties, microstructure and plane strain fracture toughness (K,,). Stres