๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Stress corrosion cracking of discontinuously reinforced aluminium (DRA) alloy 2014 during slow strain rate testing

โœ Scribed by P. M. Singh; J. J. Lewandowski


Publisher
Springer
Year
1996
Tongue
English
Weight
750 KB
Volume
15
Category
Article
ISSN
0261-8028

No coin nor oath required. For personal study only.