Poly(ether ether ketone)/poly(ether diphenyl ether ketone) blend containing 30wt% PEDEK was used to investigate the melting behaviour of immiscible PEEK/PEDEK blends. The results measured from differential scanning calorimetry (d.s.c.) and wide-angle X-ray diffraction (WAXD) showed that immiscible PEEK/PEDEK blends isothermally crystallized at a temperature between Tg and Tm2 (PEEK's normal melting point) from the glassy state also exhibited the multi-melting behaviour like poly(aryl ether ketones) homopolymers. In addition, the low-temperature melting peak was independent of composition of poly(aryl ether ketones) blends and only associated with the thermal history. ~1997 Elsevier Science Ltd.
๐ SIMILAR VOLUMES
At some given temperatures for a given time isothermally crystallized PEDEK sample exhibits two endothermic peaks which are similar to PEEK and PEEKK. The melting behavior of PEDEK crystallized from the glassy state is investigated through differential scanning calorimeter (DSC). We consider that th
## Abstract Thermal properties of poly(ether ether ketone ketone) (PEEKK)/poly(ether biphenyl ether ketone ketone) (PEDEKK) copolymers were investigated by means of differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). The glass transition temperature (__T__~g~) increases fr
## Abstract A new monomer, __N,Nโฒโ__bis(4โphenoxybenzoyl)โ__m__โphenylenediamine (BPPD), was prepared by condensation of __m__โphenylenediamine with 4โphenoxybenzoyl chloride in __N,N__โdimethylacetamide (DMAc). A series of novel poly(ether amide ether ketone) (PEAEK)/poly(ether ketone ketone) (PEK