## Abstract Potentiodynamic anodic polarization curves have been traced for an electrode of the steel Deltaβ52 (0.40, 0.78Mn, 0.045 S, 0.06P, 0.23 Si): the aggresive media used were potassium hydroxide without and with additions of potassium chloride, bromide and iodide. The oxide film present on t
The influence of heat treatment on the pitting corrosion of delta-52 steel in NaOH solutions
β Scribed by S.M. Abd El Haleem; S.S. Abd El Rehim; M.Sh. Shalaby
- Publisher
- Elsevier Science
- Year
- 1984
- Weight
- 394 KB
- Volume
- 23
- Category
- Article
- ISSN
- 0376-4583
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract A literature survey has lead to the conclusion that a theory which postulates an increased anodic reactivity on a local site in the passive film is very probable. Experiments have been set up to confirm these suggestions. By means of the electronβmicroanalyser, it is shown that CI^β^ion
## Abstract The adequacy of 7 parameters of potentiokinetic curves for evaluating the resistance to pitting corrosion in sodium chloride solutions was quantitatively assessed by reference to immersion testing in ferric chloride solutions for 11 type CrNi (MoTiCu) stainless steels on the basis of 31
High chromium martensitic steels are designed to provide high corrosion resistance in combination with high strength. Some of these steel grades contain primary carbides for improving the wear resistance, e.g. the steel 440C. The present paper mainly deals with the effect of chemical composition and