## Abstract The way in which the stationary potential of a zinc electrode previously treated with various passivating and inhibiting solutions changes in the present of the chloride, bromide and iodide ions is studied in solutions of potassium chromate, disodium hydrogen phosphate and sodium tungst
Studies on the Pitting Corrosion of the Delta-52 Steel in aqueous solutions. 2. Variation of the pitting potential in relation to the concentration of the aggressive anion
β Scribed by S. M. Abd El Haleem; S. S. Abd El Reheem; M. Sh. Shalaby; A. M. Azzam
- Publisher
- John Wiley and Sons
- Year
- 1976
- Tongue
- German
- Weight
- 764 KB
- Volume
- 27
- Category
- Article
- ISSN
- 0947-5117
No coin nor oath required. For personal study only.
β¦ Synopsis
Abstract
Potentiodynamic anodic polarization curves have been traced for an electrode of the steel Deltaβ52 (0.40, 0.78Mn, 0.045 S, 0.06P, 0.23 Si): the aggresive media used were potassium hydroxide without and with additions of potassium chloride, bromide and iodide. The oxide film present on the steel surface does not inhibit active dissolution; only at potentials exceeding+2 (S. C. E.) passivity sets in. The polarization behaviour of the steel is not influenced by the addition of the halide salts; above a certain salt concentration, however, there is a sharp increase in dissolution current. This phenomenon is an indication of the start of pitting. Between the pitting potential and the anion concentration there exists a well defined relation.
π SIMILAR VOLUMES
## Abstract A literature survey has lead to the conclusion that a theory which postulates an increased anodic reactivity on a local site in the passive film is very probable. Experiments have been set up to confirm these suggestions. By means of the electronβmicroanalyser, it is shown that CI^β^ion
## Abstract The adequacy of 7 parameters of potentiokinetic curves for evaluating the resistance to pitting corrosion in sodium chloride solutions was quantitatively assessed by reference to immersion testing in ferric chloride solutions for 11 type CrNi (MoTiCu) stainless steels on the basis of 31
## Abstract The critical pitting potential of oxide covered aluminum electrodes in aqueous chloride solutions has been investigated as a function of chloride ion concentration, temperature, solution pH and oxide film thickness. The steady state critical pitting potential decreases with chloride ion
The electrochemical behaviour of 316 stainless steel was studied in nearly neutral electrolytes containing NaCl in the -3 to 50Β°C temperature range, using potentiostatic and potentiodynamic techniques. Special attention was paid to both the current fluctuations previous to the irreversible breakdown