The effect of thermal exposure on the properties of a Ni-base superalloy

✍ Scribed by M. Aghaie-Khafri; M. Hajjavady


Publisher
Elsevier Science
Year
2008
Tongue
English
Weight
1023 KB
Volume
487
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Effect of pre-exposure on crack initiati
✍ Ali P. Gordon; Richard W. Neu; David L. McDowell πŸ“‚ Article πŸ“… 2009 πŸ› Elsevier Science 🌐 English βš– 973 KB

Blades and vanes are just two of several industrial gas turbine (IGT) components often subjected to long periods of elevated temperature before, during, and after high stress operating conditions. In these systems, cyclic loading is induced by repeated start-ups, firings, and shut-down ramps. Combin

Effects of aging treatments on the Micro
✍ Dr. Phil. W. Hoffelner; Dr. Phil. L. E. Kny; Prof. Dr. Dipl.-Ing. R. Stickler; W πŸ“‚ Article πŸ“… 1979 πŸ› John Wiley and Sons 🌐 English βš– 781 KB

## Abstract The effects of aging treatments on the microstructure of the Ni‐base superalloys IN‐738 HC and IN‐738 LC were investigated. Changes in (i) size, morphology, and distribution of the γ′‐phase, (ii) the amount of M~23~C~6~‐carbide, and (iii) the occurrence of additional phases and phase in

Hot corrosion of a plasma sprayed Ni3Al
✍ H. Singh; D. Puri; S. Prakash; T. K. Ghosh πŸ“‚ Article πŸ“… 2007 πŸ› John Wiley and Sons 🌐 German βš– 831 KB

## Abstract Ni~3~Al metallic powder was prepared by the mechanical mixing of pure nickel and aluminium powders and deposited on a Ni‐base superalloy namely Superni 75 by the shrouded plasma spray process. Hot corrosion behaviour of Ni~3~Al coated and uncoated superalloy specimens was evaluated in a

Effects of thermal exposure on the prope
✍ D.S. Lee; M.A. Stucke; D.M. Dimiduk πŸ“‚ Article πŸ“… 1995 πŸ› Elsevier Science 🌐 English βš– 998 KB

Ti-Al alloys with various alloying additions show promise as high temperature materials because of their high temperature strength and modulus. Recent strides in processing and microstructural control produced alloys which exhibit an acceptable balance of properties for aerospace applications. Howev