The effect of the tempering processes on the susceptibility to stress corrosion cracking of high strength steel

✍ Scribed by B. Pawłowski; A. Mazur; S. Gorczyca


Book ID
115847217
Publisher
Elsevier Science
Year
1991
Tongue
English
Weight
713 KB
Volume
32
Category
Article
ISSN
0010-938X