The effect of residual acetate groups on the structure and properties of vinyl alcohol–ethylene copolymers
✍ Scribed by M. L. Cerrada; R. Benavente; E. Pérez; J. M. Pereña
- Publisher
- John Wiley and Sons
- Year
- 2000
- Tongue
- English
- Weight
- 195 KB
- Volume
- 38
- Category
- Article
- ISSN
- 0887-6266
No coin nor oath required. For personal study only.
✦ Synopsis
Vinyl alcohol-ethylene (VAE) copolymers, commercially manufactured by hydrolysis of the corresponding vinyl acetate-ethylene copolymers, can contain small amounts of unhydrolyzed vinyl acetate. This article shows the influence of these residual groups on the structure of the resulting copolymers, studied by nuclear magnetic resonance and wide-angle X-ray scattering. Thermal and mechanical properties of these materials were investigated by differential scanning calorimetry, thermogravimetry, drawing behavior, birefringence measurements, and dynamic mechanical analysis. The structure of the copolymers is considerably affected by the volume of the residual acetate groups, bigger than that of the hydroxyl ones, which hinders the crystallization process. In relation to the thermal and mechanical properties, the temperature and enthalpy of melting as well as the Young's modulus and yield stress, decrease as vinyl acetate molar fraction increases. Moreover, the ␣ and  relaxations are shifted to lower temperatures as residual content in the copolymer is raised.
📜 SIMILAR VOLUMES
Temperature dependence of the complex modulus and loss tangent of the two "parent" homopolymers and three original copolymers quenched from the melt.
In order to improve the miscibility between the components of a blend, it is possible to modify the chemical structure by functionalizing one or more of the components. This results in better adhesion at the interface between the components and, consequently, in better mechanical properties. In this
Sorption isotherms of methanol, ethanol, propanol, butanol, hexanol, ethyl caproate, and limonene in 4 ethylene-vinyl alcohol (EVOH) copolymers with different ethylene contents were determined by inverse gas chromatography (IGC) at 25°C and different relative humidity conditions. From sorption isoth