Vinyl alcohol-ethylene (VAE) copolymers, commercially manufactured by hydrolysis of the corresponding vinyl acetate-ethylene copolymers, can contain small amounts of unhydrolyzed vinyl acetate. This article shows the influence of these residual groups on the structure of the resulting copolymers, st
The effect of annealing on the structure and relaxation processes of vinyl alcohol–ethylene copolymers
✍ Scribed by M. L. Cerrada; R. Benavente; E. Pérez; J. M. Pereña
- Publisher
- John Wiley and Sons
- Year
- 2000
- Tongue
- English
- Weight
- 250 KB
- Volume
- 39
- Category
- Article
- ISSN
- 0887-6266
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Temperature dependence of the complex modulus and loss tangent of the two "parent" homopolymers and three original copolymers quenched from the melt.
Sorption isotherms of methanol, ethanol, propanol, butanol, hexanol, ethyl caproate, and limonene in 4 ethylene-vinyl alcohol (EVOH) copolymers with different ethylene contents were determined by inverse gas chromatography (IGC) at 25°C and different relative humidity conditions. From sorption isoth
In this article, the synthesis and properties of the (ethylene-vinyl acetatevinyl alcohol) terpolymer are studied in detail. A transesterification reaction with alcohols was conducted on poly(ethylene-vinyl acetate) to obtain terpolymers with varying hydroxide contents through three different routes