## Abstract The effect of wood species on the mechanical and thermal properties of wood–plastic composites (WPCs) was explored. Various wood species, including cherry, sweet gum, hickory, yellow poplar, Osage orange, walnut, eastern red cedar, pine, maple, and red oak, were compounded with virgin i
The effect of crosslinker on mechanical and morphological properties of tropical wood material composites
✍ Scribed by Md. Saiful Islam; Sinin Hamdan; Md. Rezaur Rahman; Ismail Jusoh; Abu Saleh Ahmed
- Publisher
- Elsevier Science
- Year
- 2011
- Weight
- 562 KB
- Volume
- 32
- Category
- Article
- ISSN
- 0261-3069
No coin nor oath required. For personal study only.
✦ Synopsis
In this study, wood polymer composites (WPCs) based on five kinds of selected tropical wood species, namely Jelutong (Dyera costulata), Terbulan (Endospermum diadenum), Batai (Paraserianthes moluccana), Rubber (Hevea brasiliensis), and Pulai (Alstonia pneumatophora), were impregnated with methyl methacrylate (MMA) and hexamethylene diisocyanate (HMDIC) monomers mixture in the ratio of 1:1 for composite manufacturing. All these tropical wood reacted with hexamethylene diisocyanate and crosslinked with MMA which enhanced the hydrophobic (restrained water) nature of wood. The vacuum-pressure method was used to impregnate the samples with monomer mixture. The monomer mixture loading achievable was found to be dependent on the properties of wood species. Low loading was observed for the high density wood species. Mechanical strength of fabricated wood polymer composites (WPCs) in term of modulus of elasticity (MOE) and modulus of rupture (MOR) were found to be significantly improved. The wood-polymer interaction was confirmed by Fourier transform infrared (FTIR) spectroscopy. Morphological properties of raw wood and WPC samples were evaluated by scanning electron microscopy (SEM) and XRD analysis and an improvement in morphological properties was also observed for WPC.
📜 SIMILAR VOLUMES
Polypropylene/wood fiber composites were prepared at three different temperatures: 170ЊC, 180ЊC, and 190ЊC. The surface of wood fibers was modified through the use of silane coupling agents and/or coating with polypropylene or maleated polypropylene. The fiber coating was performed by propylene poly
## Abstract Effects of wood flour species and polyethylene grafted with maleic anhydride (MA‐PE) on mechanical properties and morphology and torque rheology of high density polyethylene (HDPE)/wood flour composites have been comparatively investigated. The results demonstrated that without compatbi
The mechanical properties and morphology of polypropylene/wood flour (PP/WF) composites with different impact modifiers and maleated polypropylene (MAPP) as a compatibilizer have been studied. Two different ethylene/propylene/diene terpolymers (EPDM) and one maleated styrene-ethylene/butylene-styren