## Abstract Vulcanized composites of chloroprene rubber (CR) with cellulose II (Cel II) as a filler were investigated. Cel II, obtained by the coagulation of cellulose xanthate, was incorporated in the rubber by the traditional method. The filler content varied from 0 to 30 phr. For comparison purp
The deterioration of mechanical properties of chloroprene rubber in various conditions
β Scribed by Masayuki Ito; Sohei Okada; Isamu Kuriyama
- Publisher
- Springer
- Year
- 1981
- Tongue
- English
- Weight
- 434 KB
- Volume
- 16
- Category
- Article
- ISSN
- 0022-2461
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
A systematic dielectric study over a frequency range from 400 to 10 MHz was carried out on natural rubber and chloroprene rubber with a small amount of nitroaniline additives. Three absorption regions were obtained as a result of the analysis of the curves relating dielectric loss k with frequency.
The permittivity Π and dielectric loss Π for different ratios of an ethylene propylene diene monomer (EPDM)-chloroprene rubber (CR) blend ranging from 0 to 100 phr were measured over a frequency range from 400 Hz to 60 kHz. The measurements were carried out at room temperature (25Β°C). The values of