a-Boron-containing pyrocarbons were prepared at temperatures 1400-1650°C by simultaneous pyrolytic deposition from gas mixtures containing CH, and BCI, on an induction heated graphite substrate. The deposits thus prepared with boron content in the range O-3 per cent (w/o) were investigated using X-r
Some thermomechanical properties of boron carbide and aluminum dodecaboride are presented. The dependence of the bending strength on the temperature of B 4 C and AlB 12 in the ductile rupture region was studied. It was detected that the ductile rupture of B 4 C starts at temperatures above 15003C wh