Surface Strengthening of Ti-6Al-4V Alloy by Glow Plasma Carbonization Process

✍ Scribed by Yazhe, Xing; Chaoping, Jiang; Jianmin, Hao


Book ID
123496952
Publisher
Elsevier
Year
2013
Weight
676 KB
Volume
42
Category
Article
ISSN
1875-5372

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Surface modification of Ti–6Al–4V alloy
✍ P. Budzynski; A.A. Youssef; J. Sielanko πŸ“‚ Article πŸ“… 2006 πŸ› Elsevier Science 🌐 English βš– 926 KB

Surface modification of titanium alloy (Ti-6Al-4V) by nitrogen implantation at the energy 120 keV with doses ranging from 1 Γ— 10 16 to 1 Γ— 10 18 N + /cm 2 have been investigated from the tribological point of view. Implantation of nitrogen ions was performed in two different ways: (a) when no carbon

Porous Ti-6Al-4V alloy fabricated by spa
✍ Kon, Masayuki ;Hirakata, Luciana M. ;Asaoka, Kenzo πŸ“‚ Article πŸ“… 2003 πŸ› John Wiley and Sons 🌐 English βš– 325 KB

## Abstract Porous compacts with both biological and biomechanical compatibilities and high strength were developed. Spherical powders of Ti‐6Al‐4V alloy, which were either as received or surface modified with the use of calcium ions by hydrothermal treatment (HTT), were fabricated by a spark plasm