𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Surface analysis of the initial stages of Si film growth

✍ Scribed by K. Xu; M.M. Waite; S. Ismat Shah


Publisher
Elsevier Science
Year
2004
Tongue
English
Weight
118 KB
Volume
108
Category
Article
ISSN
0921-5107

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


The kinetics of thin film island growth
✍ E. Urbonavičius; E. P≐tnyčyt≐; A. Galdikas πŸ“‚ Article πŸ“… 1999 πŸ› Elsevier Science 🌐 English βš– 101 KB

The simulation of the early stages of thin film formation is performed using a phenomenological approach considering the surface diffusion of the adatoms and the migration of islands. The model describes the kinetics of low surface coverage as well as of higher surface coverage. The effects of atom