Comparative studies of the matrix-assisted laser desorption/ionization (MALDI) of 30 antibiotics were made using a-cyano-4-hydroxycinnamic acid (HCCA), 2,5-dihydroxybenzoic acid (DHB), 5,10,15,20tetrakis(4-hydroxyphenyl)-21H,23H-porphyrin and meso-tetra(N-methyl-4-pyridyl)porphyrin matrices. Most an
β¦ LIBER β¦
Surface analysis of particles in mine tailings by time-of-flight laser-ionization mass spectrometry (TOF-LIMS)
β Scribed by C. J. Martin; T. A. Al; L. J. Cabri
- Publisher
- Springer
- Year
- 1997
- Weight
- 315 KB
- Volume
- 32
- Category
- Article
- ISSN
- 1432-0495
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Quantitative analysis of antibiotics by
β
Yong-Chien Ling; Lihnian Lin; Yi-Ting Chen
π
Article
π
1998
π
John Wiley and Sons
π
English
β 242 KB
π 2 views
Analysis of Complete Organic Semiconduct
β
Sebastian Scholz; Karsten Walzer; Karl Leo
π
Article
π
2008
π
John Wiley and Sons
π
English
β 424 KB
π 2 views
Surface enhanced laser desorptions ioniz
β
Harshadrai M. Rawel; Sascha Rohn; JΓΌrgen Kroll; Florian J. Schweigert
π
Article
π
2005
π
John Wiley and Sons
π
English
β 427 KB
Analysis of solid-supported oligonucleot
β
Albert Meyer; Nicolas Spinelli; Jean-Louis Imbach; Jean-Jacques Vasseur
π
Article
π
2000
π
John Wiley and Sons
π
English
β 134 KB
π 2 views
This study presents matrix-assisted laser desorption/ionization time-of-flight mass spectrometry (MALDI-TOFMS) as a powerful tool to analyze and characterize oligonucleotides covalently linked to a solid support during their synthesis. The analysis of the fragment ions generated either in negative o
Derivatization and Analysis of Oligosacc
β
Huan-Huan HAN; Yan MA; Lu WANG; Wan-Jun ZHANG; Jun-Ying WEI; Yang-Jun ZHANG; Xia
π
Article
π
2010
π
Elsevier Science
π
Chinese
β 543 KB
Isotopic analysis of metallic and coated
β
Inhee Choi; Kyuseok Song; Yong Joon Park; Jong-Yun Kim; Hee-Soo Yoo
π
Article
π
2010
π
Elsevier Science
π
English
β 758 KB