Treatment with superheated steam as a po
โ
Parsinson, N. ;Cuthberjson, J. W.
๐
Article
๐
1942
๐
Wiley (John Wiley & Sons)
โ 281 KB
The corrosion-resisting propcrtim of the mn~csium-nluminium-zinc nlloy A8 in the as-cast mndition can La improved by trentmcnt preferably for 1-1+ hours with supcrhosied stcam at n tempcratum of 200-280" and nt atmospheric pressure. As fatimatccl by the ealt sprny test nnd by intermittent immersion