Study of SIMS argon ion gun for quantitative surface analysis

✍ Scribed by Li Zhanping; Wang Jianhua; Li Youzhe; Chen Pijin


Book ID
104592350
Publisher
John Wiley and Sons
Year
1989
Tongue
English
Weight
397 KB
Volume
14
Category
Article
ISSN
0142-2421

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Analysis of zirconium–niobium pressure t
✍ N. S. McIntyre; C. G. Weisener; R. D. Davidson; W. N. Lennard; G. R. Massoumi; I πŸ“‚ Article πŸ“… 1990 πŸ› John Wiley and Sons 🌐 English βš– 651 KB