Stress saturation in a nickel-base superalloy, under different aging treatments

โœ Scribed by J.A del Valle; R Romero; A.C Picasso


Book ID
108467204
Publisher
Elsevier Science
Year
2001
Tongue
English
Weight
205 KB
Volume
319-321
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


In situ measurement of the lattice param
โœ A. Jacques; F. Diologent; P. Bastie ๐Ÿ“‚ Article ๐Ÿ“… 2004 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 109 KB

The evolution of the lattice parameters of the โฅ matrix and โฅ precipitates was measured in situ during high temperature tests of specimens with a raft microstructure at 1080 โ€ข C under variable load (0-300 MPa), done at the ESRF. Under low applied tensile stresses, the behavior of the specimens is pu

Prediction of crack growth in a nickel-b
โœ L.G. Zhao; J. Tong; M.C. Hardy ๐Ÿ“‚ Article ๐Ÿ“… 2010 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 851 KB

Prediction of oxidation-assisted crack growth has been carried out for a nickel-based superalloy at elevated temperature based on finite element analyses of oxygen diffusion, coupled with viscoplastic deformation, near a fatigue crack tip. The material constitutive behaviour, implemented in the fini