Stress corrosion initiated cracking of c
✍
U. Schneider; E. Nägele; F. Dumat
📂
Article
📅
1986
🏛
Elsevier Science
🌐
English
⚖ 505 KB
The simultaneous action of corrosive media and mechanical stresses on concrete leads to stress corrosion cracking phenomena. The flexural strength of mortar specimens in sulfate-solutions has been found to depend significantly on the external load being applied during the sulfatesolution exposure of