๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Stress corrosion cracking by anodic dissolution and hydrogen permeation in pipeline steels

โœ Scribed by S. Di Liberto; G. Gabetta


Book ID
110550199
Publisher
Springer
Year
1997
Tongue
English
Weight
827 KB
Volume
33
Category
Article
ISSN
1573-885X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES