Stress corrosion cracking and hydrogen embrittlement studies of austenitic and ferritic steels by small punch test

✍ Scribed by T. Misawa; Y. Hamaguchi; M. Saito


Publisher
Elsevier Science
Year
1988
Tongue
English
Weight
566 KB
Volume
155-157
Category
Article
ISSN
0022-3115

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


The effect of sulfide inclusions on the
✍ Prof. Dr. Z. Szklarska-Ε›mialowska; Dr. E. Lunarska πŸ“‚ Article πŸ“… 1981 πŸ› John Wiley and Sons 🌐 German βš– 974 KB

## Abstract Recent opinions on the effect of nonmetallic inclusions, especially sulfides, on the nucleation of pits, stress corrosion cracks, and hydrogen‐induced cracks are reviewed. The nonmetallic inclusions present in steels as impurities adversely affect the corrosion resistance of steels. Th

Report on stress-corrosion cracking of a
✍ E. Rabald πŸ“‚ Article πŸ“… 1961 πŸ› John Wiley and Sons 🌐 German βš– 159 KB

Buchbesprechungen den, das die obengenannte Aufgabenstellung erfiillt. Beriickcichtigt wurde nur in englischer Sprache erschienenes Schrifitum. Der Stoff ist in die folgenden 11 Hauptkapitel unterteilt: 1. Electrochemistry, Corrosion and Cathodic Protection 2. Practical Cathodic Protection Parameter