Stress corrosion crack of ZnAl15 alloys in hot and humid environment

โœ Scribed by Yan, Xinqi; Liu, Shengxin; Long, Weimin; Huang, Junlan; Zhang, Liangying; Chen, Yong


Book ID
121781252
Publisher
Elsevier Science
Year
2013
Tongue
English
Weight
692 KB
Volume
93
Category
Article
ISSN
0167-577X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Stress corrosion cracking of the austeni
โœ S. C. Tjong ๐Ÿ“‚ Article ๐Ÿ“… 1986 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 1011 KB

The SCC behavior of Fe-8.7A1-29.7Mn-1.04C alloy in a 20% sodium-chloride solution (100 "C) has been investigated by the slow strain rate method. The results showed that the alloy was susceptible to SCC only at the free corrosion potential and at the applied strain rate of 2.8 x lO-'/s. Application o