AbstractΓExperiments involving the indentation of single crystals of both tungsten and an iron alloy show that the observed yield phenomena can be predicted using a superdislocation model driven by the change in shear stress between the elastically and fully plastic loading conditions. A low density
Revealing deformation mechanisms with nanoindentation
β Scribed by D. Kiener; K. Durst; M. Rester; A. M. Minor
- Book ID
- 107524390
- Publisher
- The Minerals, Metals & Materials Society
- Year
- 2009
- Tongue
- English
- Weight
- 931 KB
- Volume
- 61
- Category
- Article
- ISSN
- 1047-4838
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
The deformation mechanisms of GaN thin films obtained by metal-organic chemical vapor deposition (MOCVD) method were studied using nanoindentation with a Berkovich diamond indenter, micro-Raman spectroscopy and the cross-sectional transmission electron microscopy (XTEM) techniques. Due to the sharpn
Solution and suspension thermal spraying is providing a more economic approach to the production of thin coatings. Advances in this new promising technology require accompanying tools to assess micro and nanosized areas within these deposits. Hydroxyapatite was deposited in an r.f. plasma using a po
This paper clarifies a common misunderstanding of the phase transformation in monocrystalline silicon under nanoindentation, namely that a pop-out represents the onset of a phase transition. Through a detailed investigation into the indentation-induced deformation of monocrystalline silicon using a
Nanoindentation offers a unique capability to assess the mechanical properties of polished cross-sections of thermal spray coatings. This study set out to investigate the suitability of nanoindentation to extend the analysis of the cross-section to multiple points for a more detailed insight into va