## Abstract The pitting corrosion behavior of 7150 aluminum alloy was studied by electrochemical impedance spectroscopy (EIS) in the sodium chloride and hydrochloric acid solution. Based on EIS features and corrosion morphologies as well as corrosion potential, the process of pitting corrosion coul
Relationships between microstructure and pitting corrosion of ADI in sodium chloride solution
✍ Scribed by H. Krawiec; J. Lelito; E. Tyrała; J. Banaś
- Publisher
- Springer
- Year
- 2008
- Tongue
- English
- Weight
- 465 KB
- Volume
- 13
- Category
- Article
- ISSN
- 1432-8488
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The pitting corrosion of 316 stainless steel (SS) in phosphate-borate buffer (pH 8 .00) containing 0.5 M NaCl at 25'C is studied through current transients run under a constant potential step, potentiodynamic runs and scanning electron microscopy . According to the potential and time windows differe
The localised corrosion resistance (pitting and crevice corrosion) of two high alloy stainless steels, namely superduplex (SD) and superaustenitic (SA), has been studied in chloride-fluoride solutions at pH values ranging from 2 to 6.5. The pitting potential (E pit ) and crevice potential (E cre ) h