Real time dielectric relaxation of poly(ethylene terephthalate) during crystallization from the glassy state
✍ Scribed by T.A. Ezquerra; F.J. Baltà-Calleja; H.G. Zachmann
- Book ID
- 107847022
- Publisher
- Elsevier Science
- Year
- 1994
- Tongue
- English
- Weight
- 710 KB
- Volume
- 35
- Category
- Article
- ISSN
- 0032-3861
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Poly(ethy1ene terephthalate) was crystallized from the glassy state at 120 and 200°C. The structural organization of samples, after the primary and secondary crystallizations, was analyzed by density, X-rays, infrared and transport properties of dichloromethane vapor. The values of crystallinity der
The crystallization kinetics of poly(ethy1ene terephthalate) (PET) has been studied as a function of various parameters affecting the molecular structure of the The effects of physical factors such as the previous melt history,2 additives and nucleating agents,6 the extrusion conditions,8 and orien