## Abstract Anionic polymerizations of __N__‐(4‐vinylbenzoyl)‐__N__′‐methylpiperazine (3a) and __N__‐(4‐vinylbenzoyl)morpholine (3b) were carried out in tetrahydrofuran at −78°C with oligo(α‐methylstyryl)‐dilithium, ‐disodium, and ‐dipotassium. The polymerizations of both 3a and 3b proceeded quanti
Protection and polymerization of functional monomers. 10. Synthesis of well-defined poly(4-vinylbenzaldehyde) by the anionic living polymerization of N-[(4-ethenylphenyl)methylene]cyclohexamine
✍ Scribed by Hirao, Akira; Nakahama, Seiichi
- Book ID
- 126057350
- Publisher
- American Chemical Society
- Year
- 1987
- Tongue
- English
- Weight
- 666 KB
- Volume
- 20
- Category
- Article
- ISSN
- 0024-9297
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract Anionic polymerizations of 2‐[(trimethylsilyl)oxy]ethyl methacrylate (1), 2‐[(__tert__‐butyldimethylsilyl)oxy]ethyl methacrylate (2), and 2‐[(methoxymethyl)oxy]ethyl methacrylate (3), the protected forms of 2‐hydroxyethyl methacrylate (HEMA), were carried out in THF at −78°C with 1,1‐di
## Abstract Anionic polymerization of 4‐(4′‐trimethylsilyl‐3′‐butynyl)styrene (2) was carried out in THF at −78°C for 0.5 h with oligo(α‐methylstyryl)lithium, ‐dilithium, and ‐dipotassium. Poly(2)s possessing predicted molecular weights and narrow molecular weight distributions (__M̄__~__w__~/__M̄_