The paper describes the synthesis of several polypyromellitimide samples containing phosphine oxide in the backbone and maleimido groups as pendant side chains. These polymers were obtained by solution polycondensation reaction in DMF in three steps. First step involved the reaction of equimolar amo
Properties of polypyromellitimides containing phosphorus
β Scribed by I. K. Varma; Ramakant Kumar; Sneh Saxena; D. S. Varma
- Publisher
- John Wiley and Sons
- Year
- 1991
- Tongue
- English
- Weight
- 409 KB
- Volume
- 42
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
β¦ Synopsis
The paper deals with the synthesis and characterization of seven polypyromellitimide samples having varying contents of phosphine oxide and ether linkages in the backbone with pendant maleimido groups. Curing characteristics and thermal stability of polymers were evaluated by differential scanning calorimetry and dynamic thermogravimetry. It was observed that an increase in pendant maleimido groups resulted in an increase in the heat of polymerization. Char yield also increased with increase in phosphorus content. Conductivity and dielectric parameters were also evaluated. The mechanism of conduction was found to be a combination of electronic and ionic type.
π SIMILAR VOLUMES
A series of advanced epoxy resins with various epoxy equivalent weights were synthesized from a reactive phosphorus-containing diol, 2-(6-oxido-6Hdibenz[c,e][1,2]oxaphosphorin-6-yl)-1,4-dihydroxy phenylene and diglycidyl ether of bisphenol A and then cured with 4,4Π-diaminodiphenyl sulfone, phenol n
## Abstract ChemInform is a weekly Abstracting Service, delivering concise information at a glance that was extracted from about 100 leading journals. To access a ChemInform Abstract of an article which was published elsewhere, please select a βFull Textβ option. The original article is trackable v
Chemical vapour codeposition of carbon and phosphorus was effected from a CH4 + PC&+ H2 gas mixture at deposition temperatures ranging from 1220" to 1730Β°C. fin a total gas pressure of 133 mbar and with I-15 vol '% PCl:% in the gas mixture. The product of the codeposition is a pyrocarbon containing