Pressureless-sintered and HIPed SiC-TiB2composites from SiC-TiO2-B4C-C powder compacts

✍ Scribed by Toshihiko Tani; Shigetaka Wada


Publisher
Springer
Year
1991
Tongue
English
Weight
798 KB
Volume
26
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Processing and characterization of B4C–S
✍ Manish Patel; J. Subrahmanyam; V.V. Bhanu Prasad; Rajnish Goyal πŸ“‚ Article πŸ“… 2010 πŸ› Elsevier Science 🌐 English βš– 720 KB

B 4 C-SiC-Si-TiB 2 composites were synthesized by a two step process. TiB 2 particles in the size range 2-5 m were generated in situ in the first step and were distributed in the residual silicon present in the reaction bonded boron carbide, in the second step. The composites were characterized by X

Thermal decomposition, densification and
✍ Sea-Hoon Lee; Shuqi Guo; Hidehiko Tanaka; Kenji Kurashima; Toshiyuki Nishimura; πŸ“‚ Article πŸ“… 2008 πŸ› Elsevier Science 🌐 English βš– 759 KB

Thermal decomposition of AlN-SiC(-TiB 2 ) systems during densification was analyzed, and effects of B, B 4 C and C on the densification behavior of the systems were studied. SiO 2 impurity in the powder mixture was nearly completely removed by carbothermal reaction at 1500 β€’ C in vacuum, while Al 2

Thermal shock behavior of as-sintered an
✍ Guiqing Chen; Rubing Zhang; Hao Zou πŸ“‚ Article πŸ“… 2010 πŸ› Elsevier Science βš– 571 KB

A water-quenching technique was adopted to evaluate the thermal shock behavior of as-sintered and pre-oxidation Zr 2 Al 4 C 5 -20 vol.%SiC composites in an air atmosphere. The strength retention of the two kinds of composites was measured after varying temperature (DTc) up to 800 Β°C. As-sintered Zr