✦ Synopsis
Olive stones have been carbonized under a flow of nitogen in the temperature range from 700 to 900°C and activated in a CO2 flow in the range from 675 to 875°C. ZnCI, was used in some of the activation processes.
The adsoptive characteristics of the carbonized and activated samples have been determined by adsorption of nitrogen (77 and 90 K), carbon dioxide (195 and 273 K), n-butane (273 K) and methylene blue (aqueous solution at 298 K). Meso and macroporosity have been followed by mercury porosimetry. The resulting activated carbons have very large surface areas as well as a highly developed microporosity. The most adequate experimental conditions for the preparation of active carbons, highly microporous but with a well developed meso and macroDorosity, are discussed. All active carbons prepared have a very low ash content and complete absence of sulphir, both-very attractive characteristics.
📜 SIMILAR VOLUMES
## Abstract Activated carbons were prepared from olive oil solid wastes by treatment in different schemes: impregnation with H~3~PO~4~ followed by pyrolysis at 300–700 °C, by steam pyrolysis at 600–700 °C, or by conventional steam activation at 850 °C. Porosity characteristics were determined by an
Preparation of activated carbons from eucalyptus kraft lignin has been investigated. A pretreatment method has been established to avoid partial fusion and swelling in the carbonization stage. Carbonization has been studied at different temperatures and the structure of the microporous chars has bee
Powdered activated carbon has been prepared from lignitic coal of Lakhra (Pakistan) by a chemical activation method using ZnCl, as an activating agent. Different process variables have been established after a series of experiments and an impregnation ratio of 1: 2, an activation temperature of 650°
## Abstract The polymeric precursor polystyrene sulphonate beads were used to produce activated carbon spheres (ACSs). ACSs were prepared by carbonization of polymeric precursor at 800°C followed by activation of resultant char with steam and carbon dioxide activation processes. The resulting ACSs