Pitting Corrosion Characteristics of Aluminum - Influence of Magnesium and Manganese.

✍ Scribed by Aziz, P. M.; Godard, Hugh P.


Book ID
120326027
Publisher
American Chemical Society
Year
1952
Weight
686 KB
Volume
44
Category
Article
ISSN
0019-7866

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Corrosion Behaviour of Manganese-Contain
✍ A. M. Shams El Din; M. M. Badran; S. E. Khalil πŸ“‚ Article πŸ“… 1973 πŸ› John Wiley and Sons 🌐 German βš– 452 KB

## Abstract The pitting susceptibility of stainless steels with (%) 17.39 Cr, 5.3 Ni, 0.3–13.9 Mn in chloride solutions have been studied by a potentiodynamic cyclic polarization technique in solutions 0.1 N H~2~SO~4~ + 0.9 N Na~2~So~4~ + various amounts of NaCl. At low NaCl concentrations no prono

Multiscale characterization of pitting c
✍ George N. Frantziskonis; Laura B. Simon; Jung Woo; Theodore E. Matikas πŸ“‚ Article πŸ“… 2000 πŸ› Elsevier Science 🌐 English βš– 204 KB

This paper documents a novel method for characterizing pitting corrosion damage in structural materials such as Al 2024-T3. Specimens of such alloys are corroded in a controlled environment and the pits' geometry is captured digitally using white light interference microscopy. The digital data are t