A novel liquid wicking process has been developed to produce silver-sheathed Bi-2212 samples with oxide core thicknesses of 10-20 p~m, uniform oxide/silver interfaces, small non-superconducting phases and low porosity. This technique avoids many problems associated with oxide-powder-in-tube (OPIT) p
The tensile mechanical property and the axial tensile strain/transverse compressive stress dependence of the critical current I c in mono-and 19-core Bi(2212) superconducting tapes with Zr-reinforced Ag sheaths were evaluated at a temperature of 4.2 K and a magnetic field of 14 T. Replacement of Ag