𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Phase chemistry of a nickel-base superalloy after creep experiments

✍ Scribed by Schmidt, R.; Feller-Kniepmeier, M.


Book ID
123221580
Publisher
Elsevier Science
Year
1993
Weight
498 KB
Volume
29
Category
Article
ISSN
0956-716X

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Microstructure of a nickel-base superall
✍ Thomas Kuttner; Monika Feller-Kniepmeier πŸ“‚ Article πŸ“… 1994 πŸ› Elsevier Science 🌐 English βš– 718 KB

Tensile creep tests in the [011] direction have been performed on two specimens of SRR99 at 1173 K under a load of 300 MPa. The microstructure was analysed by transmission electron microscopy investigations after plastic strains of 0.1% and 0.29%. At both strains, the 7' phase is not sheared by disl

Creep of PE-10 nickel-base superalloy at
✍ A. J. Marzocca; A. C. Picasso πŸ“‚ Article πŸ“… 1994 πŸ› Springer 🌐 English βš– 853 KB

Creep data, at 973 K and stresses between 355 and 512 MPa, in flat specimens of PE-IO nickel-base superalloy are reported. The data have been interpreted in terms of a constitutive equation based on a creep model involving dislocation climb and cross-slip over the strengthening phase. Strain-rate se