✦ Synopsis
Oxazoline functionality is well known to be highly reactive toward a lot of other functional groups like carboxyls, hydroxyls, mercaptans, and amines. In this work we report the possibility to modify the nitrile groups of an acrylonitrile/butadiene/ styrene (ABS) copolymer into oxazoline in the molten state in the presence of aminoethanol as modifier agent and zinc acetate as a catalyst. The reaction has been carried out in a batch mixer and in a corotating twin screw extruder. The conversion of the nitrile groups into oxazoline has been verified by infrared spectroscopy, NMR analysis microanalysis and confirmed by thermomechanical characterization. The results indicate that the kinetic of grafting is fast and the conversion of the nitrile groups into oxazoline relatively high, encouraging the use of this modified polymer in the reactive compatibilization of ABS-based blends.
📜 SIMILAR VOLUMES
## Abstract The graft copolymerization of maleic anhydride (MAH) onto acrylonitrile–butadiene–styrene terpolymer (ABS) was carried out with dicumyl peroxide (DCP) and benzoyl peroxide (BPO) as the binary initiators and with styrene as the comonomer in the molten state. IR spectra confirmed that MAH
## Abstract The graft copolymerization of maleic anhydride (MAH) onto acrylonitrile‐butadiene‐styrene terpolymer (ABS) using dicumyl peroxide and benzoyl peroxide as the binary initiator and styrene as the comonomer in the molten state was described. The properties and phase morphologies of the mod
## Abstract Critical strains causing environmental stress cracking of injection‐molded poly(acrylonitrile‐butadiene‐styrene) (ABS) and poly(styrene‐acrylonitrile) (SAN) plaques were determined upon exposure to methanol. Measurements were obtained for samples strained either parallel or perpendicula