Challenges in modelling the evolution of
โ
A. Turnbull; D.A. Horner; B.J. Connolly
๐
Article
๐
2009
๐
Elsevier Science
๐
English
โ 607 KB
The evolution of stress corrosion cracks from pits is important in many industrial applications but continues to be a challenge in both measurement and prediction. Life prediction in these circumstances has to account for pit growth kinetics, the conditions for the transition from pits to cracks, an