𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Challenges in modelling the evolution of stress corrosion cracks from pits

✍ Scribed by A. Turnbull; D.A. Horner; B.J. Connolly


Publisher
Elsevier Science
Year
2009
Tongue
English
Weight
607 KB
Volume
76
Category
Article
ISSN
0013-7944

No coin nor oath required. For personal study only.

✦ Synopsis


The evolution of stress corrosion cracks from pits is important in many industrial applications but continues to be a challenge in both measurement and prediction. Life prediction in these circumstances has to account for pit growth kinetics, the conditions for the transition from pits to cracks, and the growth rate of cracks in the short and long crack domain. An example of importance is the performance of steam turbine rotors in power generation. Although stress corrosion failures are comparatively rare, the consequences can be severe and occasionally catastrophic. Consequently, considerable effort is being focused on evaluating the effect of operational variables on pitting and crack growth and in developing an improved basis for structural integrity assessment. A preliminary mathematical model based on deterministic equations with statistically variable input parameters was developed for simulating the evolution of the pit depth distribution at different exposure times, and the transformation to stress corrosion cracks was based on the Kondo criteria. The model predicted some features of the damage well but recent novel measurements of the evolution of stress corrosion cracks from pits combined with finite element analysis of the strain distribution suggest that the transition from a pit to a crack is more complex than can be accounted for by the Kondo approach.


πŸ“œ SIMILAR VOLUMES


The significance of stress corrosion cra
✍ D. Rhodes; J.K. Musuva; J.C. Radon πŸ“‚ Article πŸ“… 1981 πŸ› Elsevier Science 🌐 English βš– 1005 KB

Abslraet-A model is proposed to account for interactions between fatigue and stress corrosion crack propagation mechanisms in appropriate corrosion fatigue conditions. Tests on an alloy steel, and both wrought and cast aluminium alloys, are reported. Despite the use of very simple coefficients in th

Early stages in the development of stres
✍ R.H. Jones; E.P. Simonen πŸ“‚ Article πŸ“… 1994 πŸ› Elsevier Science 🌐 English βš– 773 KB

Processes involved in the growth of short cracks and stage I of long stress corrosion cracks have been identified and evaluated. There is evidence that electrochemical effects can cause short stress corrosion cracks to grow at rates which are either faster or slower than those of long cracks. Short

Simulation of hydrogen assisted stress c
✍ I. Scheider; M. Pfuff; W. Dietzel πŸ“‚ Article πŸ“… 2008 πŸ› Elsevier Science 🌐 English βš– 241 KB

This paper investigates the effect of hydrogen diffusion on stable crack propagation by using numerical finite element simulations based on the cohesive model. The model with its two common parameters, cohesive strength, T 0 , and critical separation, d 0 , and its two additional parameters for stre

Theoretical description of the practical
✍ S. Wang πŸ“‚ Article πŸ“… 2005 πŸ› John Wiley and Sons 🌐 German βš– 97 KB

Stress corrosion cracking (SCC) from crevice corrosion sites had been found in an experimental work at polarization potential of ΓΎ 200 mV SCE . In that work, an occluded U-bend specimen of Type 316L (UNS S31603) stainless steel was used. The testing was done in sodium chloride (NaCl) solution. Based

The effect of sulfide inclusions on the
✍ Prof. Dr. Z. Szklarska-Ε›mialowska; Dr. E. Lunarska πŸ“‚ Article πŸ“… 1981 πŸ› John Wiley and Sons 🌐 German βš– 974 KB

## Abstract Recent opinions on the effect of nonmetallic inclusions, especially sulfides, on the nucleation of pits, stress corrosion cracks, and hydrogen‐induced cracks are reviewed. The nonmetallic inclusions present in steels as impurities adversely affect the corrosion resistance of steels. Th