Modeling the hot-deformation behavior of Ni60 wt%–Ti40 wt% intermetallic alloy

✍ Scribed by A.A. Khamei; K. Dehghani


Book ID
116605702
Publisher
Elsevier Science
Year
2010
Tongue
English
Weight
721 KB
Volume
490
Category
Article
ISSN
0925-8388

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Effect of α-precipitation on the superel
✍ R. Arockiakumar; J.K. Park 📂 Article 📅 2010 🏛 Elsevier Science 🌐 English ⚖ 510 KB

A ultrafine-grain-structured Ti-40Nb-0.3O (wt.%) alloy has been fabricated via equal channel angular extrusion (ECAE) followed by annealing within an ␣ + ␤ two-phase field. The precipitation of ␣-phase was responsible for producing an annealed ultrafine-grain structure of about 1 m. As-ECAEed specim

Effect of conventional and subzero treat
✍ S.Hossein Nedjad; M Nili-Ahmadabadi; R Mahmudi; H Farhangi 📂 Article 📅 2004 🏛 Elsevier Science 🌐 English ⚖ 242 KB

Fe-Ni-Mn maraging alloys are suffering from sever embrittlement after aging. Mechanism of the embrittelement has not been well understood yet. Segregation of Mn atoms or formation of Austenite particles at prior Austenite grain boundaries (PAGBs) have been reported as embrittelement mechanisms while