✦ Synopsis


The intrinsic viscosity of polystyrene-poly(ethylene oxide) (PS-PEO) and PS-poly(ethylene glycol) (PEG) blends have been measured in benzene as a function of blend composition for various molecular weights of PEO and PEG at 303.15 K. The compatibility of polymer pairs in solution were determined on the basis of the interaction parameter term, Db, and the difference between the experimental and theoretical weight-average intrinsic viscosities of the two polymers, D[h]. The theoretical weightaverage intrinsic viscosities were calculated by interpolation of the individual intrinsic viscosities of the blend components. The compatibility data based on [ h] determined by a single specific viscosity measurement, as a quick method for the determination of the intrinsic viscosity, were compared with that obtained from [ h] determined via the Huggins equation. The effect of molecular weights of the blend components and the polymer structure on the extent of compatibility was studied.


πŸ“œ SIMILAR VOLUMES


Biodegradability of Poly(ethylene tereph
✍ Nagata, Minoru; Kiyotsukuri, Tsuyoshi; Minami, Susumu; Tsutsumi, Naoto; Sakai, W πŸ“‚ Article πŸ“… 1996 πŸ› John Wiley and Sons 🌐 English βš– 400 KB πŸ‘ 1 views

Poly(ethy1ene terephthalate) copolymers were prepared by melt polycondensation of dimethyl terephthalate and excess ethylene glycol with 10- 40 mol% (in feed) of poly(ethy1ene glycol) (E) and poly(tetramethy1ene glycol) (B), with molecular weight (MW) of E and B 200-7500 and 1000, respectively. The

Surface modification of poly(ethylene te
✍ Fusako Seto; Akio Kishida; Yoichiro Muraoka; Mitsuru Akashi πŸ“‚ Article πŸ“… 1999 πŸ› John Wiley and Sons 🌐 English βš– 161 KB πŸ‘ 1 views

The poly(ethylene glycol) (PEG)-grafted styrene (St) copolymer, which was formed as a nanosphere, was used as an agent to modify the surface of poly(ethylene terephthalate) (PET) film. The graft copolymer was dissolved into chloroform and coated onto the PET film by dip-coating method. The coated am

Crystallization of poly(ethylene oxide)
✍ T. Kowalewski; G. Ragosta; E. Martuscelli; A. Galeski πŸ“‚ Article πŸ“… 1997 πŸ› John Wiley and Sons 🌐 English βš– 294 KB πŸ‘ 1 views

A two-stage stable system of isotactic polypropylene-poly(ethylene oxide) blend, in which poly(ethylene oxide) can be permanent either in molten or in crystallized states in the temperature range from 280 to 327 K, was described. The behavior of that blend was explained in terms of fractionated crys

Poly(ester–carbonates) containing poly(l
✍ Maurizio Penco; Michele Becattini; Paolo Ferruti; Salvatore D'antone; Ramano Deg πŸ“‚ Article πŸ“… 1996 πŸ› John Wiley and Sons 🌐 English βš– 486 KB

The aim of the present paper is to report on the synthesis, characterization and structure-property relationships of a novel family of highly hydrophilic segmented copoly (esterether-carbonafes). The synthetic process is based on a chain-extension reaction involving low molecular weight poly(1actic-