The mechanical properties of non-vulcanized natural rubber and dialyzed natural rubber-clay nanocomposites have been studied by uniaxial deformations to evaluate the reinforcement efficiency of the clay. We show that while non-rubber molecules contribute to auto-reinforcement, removal of these molec
Mill processing and properties of rubber–clay nanocomposites
✍ Scribed by M. Nadeem Qureshi; H. Qammar
- Publisher
- Elsevier Science
- Year
- 2010
- Tongue
- English
- Weight
- 796 KB
- Volume
- 30
- Category
- Article
- ISSN
- 0928-4931
No coin nor oath required. For personal study only.
✦ Synopsis
The dispersion of nanoscale composites in elastomers, which generally have higher molecular weight and viscosity as compared to plastics, is a challenge. Several techniques have been proposed for improvement of the dispersion of nanofillers in the polymers [1]. For example, the interaction of natural layered silicates can be improved by ion-exchange of hydrated cation with organic cations such as introducing bulky alkylammoniums to obtain larger interlayer spacing and provide the galleries for the polymer chain diffusion. The resultant swollen nanoclay was dried and dispersed in the polymer matrix by means of high shear mixers [2][3]. In this paper we describe the results from a new method of incorporating nanofillers into solid rubber by use of a conventional two-roll mill, which we call the modified mill method. The properties of the resultant material are compared with that of the material prepared by a latex method. We also test processability parameters, tensile behavior and crosslink density of carbon black composites prepared by the same two methods to provide a comparison between the nanocomposites. The rubber-clay nanocomposites prepared by the mill method are shown to have a fine dispersed phase structure and good reinforcement properties.
📜 SIMILAR VOLUMES
## Abstract In this work, polypropylene/clay nanocomposites with 0.5, 1, 3, and 5 wt % of montmorillonite (MMT) (unmodified clay) were prepared by intensive mixing at 50 rpm and 10 min of mixing. For the highest clay content (5 wt %), the initial materials or the processing conditions were changed