Microstructures of a single-crystal nickel-base superalloy after thermo-mechanical fatigue

✍ Scribed by Wang, Y. C.; Li †, S. X.; Zhou, L.; Ai, S. H.; Liu, F.; Zhang, H.; Wang, Z. G.


Book ID
125814552
Publisher
Taylor and Francis Group
Year
2004
Tongue
English
Weight
732 KB
Volume
84
Category
Article
ISSN
1478-6435

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Thermo-mechanical fatigue failure of a s
✍ M. Okazaki; M. Sakaguchi 📂 Article 📅 2008 🏛 Elsevier Science 🌐 English ⚖ 480 KB

Behavior of thermo-mechanical fatigue (TMF) of a single crystal Ni-based superalloy, CMSX-4, was studied, compared with that of isothermal low cycle fatigue (LCF). Strain-controlled TMF and LCF tests of CMSX-4 were carried out under various test conditions, where the experimental variables were stra